THE ENGINEERING QUALITY SUPPORT FOR THE SILICON CARBIDE RING'S EDGES WHICH ARE THE FRICTION PAIR OF THE PUMP'S FACE SEAL
https://doi.org/10.17073/1683-4518-2017-11-65-69
Abstract
The formation morphology characteristics studying of the SiSIC-ceramics samples edges in course of the diamond grinding allowed to define the basic kinds of crumbling and their geometrical parameters. The correlation was revealed between the grinding depth, the longitudinal and transverse motions and the crumbling geometrical parameters. Ill. 5. Ref. 19.
About the Authors
V. V. KuzinRussian Federation
S. Yu. Fedorov
Russian Federation
S. N. Grigoriev
Russian Federation
References
1. Баткис, Г. С. Торцовые уплотнения нового поколения для центробежных и винтовых компрессоров / Г. С. Баткис, Н. М. Лившиц, В. К. Хайсанов [и др.] // Вестник казанского технологического университета. ― 2010. ― № 9. ― С. 408‒417.
2. Кириллов, Н. П. Конструкции торцовых уплотнений для вращающихся валов центробежных насосов систем заправки ракет / Н. П. Кириллов, В. В. Буренин, В. И. Полянский [и др.] // Вестник московского автомобильно-дорожного государственного технического университета (МАДИ). ― 2012. ― № 1. ― С. 18‒22.
3. Голубев, А. И. Торцевые уплотнения вращающихся валов / А. И. Голубев. ― М. : Машиностроение, 1974. ― 212 с.
4. ОСТ 26-06-1493‒87. Уплотнения торцовые валов насосов. Типы. Основные параметры и размеры.
5. Душко, О. В. Композиционные износостойкие материалы на основе карбида кремния / О. В. Душко, А. П. Уманский, Д. О. Пушкарев // Огнеупоры и техническая керамика. ― 2005. ― № 2. ― С. 22‒24.
6. Параносенков, В. П. Конструкционные материалы на основе самосвязанного карбида кремния / В. П. Параносенков, А. А. Чикина, М. А. Андреев // Огнеупоры и техническая керамика. ― 2006. ― № 7. ― С. 37‒40.
7. Кузин, В. В. Взаимосвязь режимов алмазного шлифования с состоянием поверхности SiSiC-керамики / В. В. Кузин, С. Ю. Фёдоров, С. Н. Григорьев // Новые огнеупоры. ― 2017. ― № 3. ― С. 179‒185.
8. Kuzin, V. V. Correlation of diamond grinding regimes with SiSiC-ceramic surface condition journal / V. V. Kuzin, S. Yu. Fedorov, S. N. Grigor’ev // Refractories and Industrial Ceramics. ― 2017. ― Vol. 58, № 2. ― Р. 214‒219.
9. Dai, Jianboi. The influence of grain geometry and wear conditions on the material removal mechanism in silicon carbide grinding with single grain / Jianbo Dai, Honghua Su, Hao Hu [et al.] // Ceramics International. ― 2017. ― Vol. 43, № 15. ― P. 11973‒11980.
10. Agarwal, Sanjay. Optimizing machining parameters to combine high productivity with high surface integrity in grinding silicon carbide ceramics / Sanjay Agarwal // Ceram. Int. ― 2016. ― Vol. 42, № 15. ― P. 6244‒6262.
11. Kuzin, V. A model of forming the surface layer of ceramic parts based on silicon nitride in the grinding process / V. Kuzin // Key Engineering Materials. ― 2012. ― Vol. 496. Precision Machining. ― Р. 127‒131.
12. Zhang, Quanli. Surface generation mechanism of WC/Co and RB‒SiC/Si composites under high spindle speed grinding (HSSG) / Quanli Zhang, Suet To, Qingliang Zhao [et al.] // Int. J. Refract. Met. Hard Mater. ― 2016. ― Vol. 56. ― P. 123‒131.
13. Cao, Jianguo. Material removal behavior in ultrasonicassisted scratching of SiC ceramics with a single diamond tool / Jianguo Cao, Yongbo Wu, Dong Lu [et al.]// International Journal of Machine Tools and Manufacture. ― 2014. ― Vol. 79. ― P. 49‒61.
14. Душко, О. В. Алмазное шлифование карбидокремниевой керамики для машиностроения / О. В. Душко, В. М. Шумячер. ― Волгоград : ВолгГАСУ, 2009. ― 80 с.
15. Zhang, Quanli. Amorphization and segregation based surface generation of reaction-bonded Si/SiC composites under micro grinding / Quanli Zhang, Suet To, Qingliang Zhao [et al.]// International Journal of Machine Tools and Manufacture. ― 2015. ― Vol. 95. ― P. 78‒81.
16. Kuzin, V. Designing of detailstaking into account degradation of structural ceramics at exploitation / V. Kuzin, S. Grigoriev, M. Volosova, M. Fedorov // Applied Mechanics and Materials. ― 2015. ― Vols. 752/753. ― Р. 268‒271.
17. Kuzin, V. Surface defects formation in grinding of silicon nitride ceramics / V. Kuzin, S. Grigoriev, S. Fedorov, M. Fedorov // Applied Mechanics and Materials. ― 2015. ― Vols. 752/753. ― Р. 402‒406.
18. Кузин, В. В. Закономерности формирования морфологии кромок образцов Al2O3‒TiC-керамики при алмазном шлифовании / В. В. Кузин, С. Ю. Фёдоров, С. Н. Григорьев // Новые огнеупоры. ― 2017. ― № 5. ― С. 63‒67.
19. Kuzin, V. V. Features of Al2O3–TiC-ceramic specimen edge morphology formation during diamond grinding / V. V. Kuzin, S. Yu. Fedorov, S. N. Grigor’ev // Refractories and Industrial Ceramics. ― 2017. ― Vol. 58, № 3. ― Р. 319‒323.
20. Кузин, В. В. Закономерности формирования морфологии кромок образцов Y‒TZP-керамики при алмазном шлифовании / В. В. Кузин, С. Ю. Фёдоров, С. Н. Григорьев // Новые огнеупоры. ― 2017. ― № 7. ― С. 63‒65.
21. Кузин, В. В. Уровень дефектности кромок образцов Si3N4-керамики после алмазного шлифования / В. В. Кузин, С. Ю. Фёдоров, С. Н. Григорьев // Новые огнеупоры. ― 2017. ― № 9. ― С. 65‒68.
Supplementary files
For citation: Kuzin V.V., Fedorov S.Y., Grigoriev S.N. THE ENGINEERING QUALITY SUPPORT FOR THE SILICON CARBIDE RING'S EDGES WHICH ARE THE FRICTION PAIR OF THE PUMP'S FACE SEAL NOVYE OGNEUPORY (NEW REFRACTORIES). 2017;(11):65-69. https://doi.org/10.17073/1683-4518-2017-11-65-69
Refbacks
- There are currently no refbacks.