THE DEFECT RATE OF THE Y‒TZP-CERAMIC SAMPLE EDGES AFTER DIAMOND GRINDING
https://doi.org/10.17073/1683-4518-2017-7-63-65
Abstract
On the minimal TiB2 ontent in the alumina-wetted cathode composite.
On base of the edges morphology forming specifics investigation for the Y‒TZP-ceramic samples in the course of diamond grinding the chunking out main kinds and geometrical parameters were defined. The interrelation between the grinding depth, the transverse and longitudinal motions and the chunking out geometrical parameters were established. Ill. 3. Ref. 2.
About the Authors
V. V. KuzinRussian Federation
S. Yu. Fedorov
Russian Federation
S. N. Grigoriev
Russian Federation
References
1. Кузин, В. В. Взаимосвязь режимов алмазного шлифования с состоянием поверхности керамики на основе диоксида циркония / В. В. Кузин, С. Ю. Фёдоров, С. Н. Григорьев // Новые огнеупоры. ― 2016. ― № 11. ― С. 60‒65. Kuzin, V. V. Correlation of diamond grinding regime with surface condition of ceramic based on zirconium dioxide / V. V. Kuzin, S. Yu. Fedorov, S. N. Grigor’ev // Refractories and Industrial Ceramics. ― 2017. ― Vol. 57, № 6. ― P. 625‒630.
2. Кузин, В. В. Закономерности формирования морфологии кромок образцов Al2O3 ‒TiC-керамики при а лмазном ш лифовании / В. В. Кузин, С. Ю. Фёдоров, С. Н. Григорьев // Новые огнеупоры. ― 2017. ― № 5. ― С. 63‒67.
Supplementary files
For citation: Kuzin V.V., Fedorov S.Y., Grigoriev S.N. THE DEFECT RATE OF THE Y‒TZP-CERAMIC SAMPLE EDGES AFTER DIAMOND GRINDING. NOVYE OGNEUPORY (NEW REFRACTORIES). 2017;(7):63-65. https://doi.org/10.17073/1683-4518-2017-7-63-65
Refbacks
- There are currently no refbacks.