Temperature coefficient of linear expansion of glass-ceramic materials based on MoSi2


https://doi.org/10.17073/1683-4518-2023-7-38-41

Full Text:




Abstract

The influence of temperature-time parameters on the temperature coefficient of linear expansion (TCLR) of materials based on MoSi2‒B‒Al2O3 has been established. It is shown that by changing the composition of the composition and the conditions of heat treatment, it is possible to significantly influence the value of TCLR.


About the Authors

I. B. Ban’kovskaya
ФГБУН «Институт химии силикатов имени И. В. Гребенщикова РАН»
Russian Federation


D. V. Kolovertnov
ФГБУН «Институт химии силикатов имени И. В. Гребенщикова РАН»
Russian Federation


M. V. Sazonova
ФГБУН «Институт химии силикатов имени И. В. Гребенщикова РАН»
Russian Federation


References

1. Щурик, А. Г. Искусственные углеродные материалы / А. Г. Щурик. ― Пермь : Изд.-во Перм. гос. ун-та, 2009. ― 342 с.

2. Niu, Y. R. Comparison of ZrB2‒MoSi2 composite coatings fabricated by atmospheric and vacuum plasma spray processes / Y. R. Niu, Z. Wang, J. Zhao [et al.] // J. Therm. Spray Technol. ― 2017. ― № 26. ― P. 100‒107.

3. Zhang, Y. L. C/SiC/ Si‒Mo‒B/glass multilayer oxidation protective coating for carbon/carbon composites / Y. L. Zhang, H. J. Li, X. Y. Yao [et al.] // Surf. Coat. Technol. ― 2011. ― № 206. ― P. 492‒496.

4. Feng, T. Microstructure and oxidation of multilayer MoSi2‒CrSi2‒Si coatings for SiC coated carbon/carbon composites SiC internal layer / T. Feng, H. J. Li, Q. G. Fu [et al.] // Corros. Sci. ― 2010. ― № 52. ― P. 3011‒3017.

5. Li, T. Effect of LaB6 on the thermal shock property of MoSi2‒SiC coating for carbon/carbon composites / T. Li, H. J. Li, X. H. Shi // Appl. Surf. Sci. ― 2013. ― № 264. ― P. 88‒93.

6. Сазонова, М. В. Термическая стабильность композитов и покрытий на основе MoSi2‒B‒Al2O3 при нагревании на воздухе до 1600 o С / М. В. Сазонова, И. Б. Баньковская, Д. В. Коловертнов // Новые огнеупоры. ― 2021. ― № 11. ― С. 48‒51.

7. Kolovertnov, D. V. Effect of temperature ― time parameters on the structure and properties of glass-ceramic composites based on molybdenum disilicide / D. V. Kolovertnov, I. B. Ban’kovskaya, M. V. Sazonova // Glass Phys. Chem. ― 2022. ― Vol. 48, № 6. ― P. 642‒645.

8. Клюев, В. П. Тепловое расширение и температура стеклования кальциевоборатных и кальциевоалюмоборатных стекол / В. П. Клюев, Б. З. Певзнер // Физика и химия стекла. ― 2003. ― Т. 29, № 2. ― С. 191‒204.

9. Wu, H. Effect of spraying power on microstructure and bonding strength of MoSi2-based coatings prepared by supersonic plasma spraying / H. Wu, H. J. Li, Q. Lei [et al.] // Appl. Surf. Sci. ― 2011. ― № 257. ― Р. 5566–5570.

10. Wang, C. C. Oxidation behavior and microstructural evolution of plasma sprayed La2O3‒MoSi2‒SiC coating on carbon/carbon composites / C. C. Wang, K. Z. Li, C. X. Huo [et al.] // Surf. Coat. Technol. ― 2018. ― № 348. ― P. 81‒90.

11. Chen, Peng. Preparation of oxidation protective MoSi2‒SiC coating on graphite using recycled waste MoSi2 by one-step spark plasma sintering method / Peng Chen, Lu Zhu, Xuanru Ren [et al.] // Ceram. Int. ― 2019. ― № 45. ― P. 22040—22046.

12. Николаев, А. Н. Синтез и исследование свойств жаростойких покрытий на основе композиции Si‒ B4C‒ZrB2‒ZrO2 / А. Н. Николаев, И. Б. Баньковская, Д. В. Коловертнов // Физика и химия стекла. ― 2020. ― Т. 46, № 6. ― С. 649‒657.

13. Silvestroni, Laura. Method to improve the oxidation resistance of ZrB2-based ceramics for reusable space systems / Laura Silvestroni, Simone Failla, Irina Neshpo, Oleg Grigoriev // J. Eur. Ceram. Soc. ― 2018. ― № 38. ― P. 2467‒2476.

14. Zhang, Н. A novel microstructural design to improve the oxidation resistance of ZrB2‒SiC ultra-high temperature ceramics (UHTCs) / H. Zhang, D. D. Jayaseelan, I. Bogomol [et al.] // J. Alloys Compounds. ― 2019. ― № 785. ― P. 958‒964.

15. Баньковская, И. Б. Термическая стабильность композиций из дисилицида молибдена, кварца и стекла. Антикоррозионные покрытия : тр. 10-го Всесоюз. совещания по жаростойким покрытиям, Ленинград, 12‒14 мая 1981 г. / И. Б. Баньковская, М. В. Сазонова. ― Л. : Наука, 1983. ― С. 50‒57.

16. Баньковская, И. Б. Развитие работ по созданию покрытий для защиты углеродных материалов при высоких температурах (oбзор по работам ИХС РАН) / И. Б. Баньковская, Д. В. Коловертнов // Физика и химия стекла. ― 2017. ― Т. 43, № 2. ― С. 156‒171.

17. Малышев, В. В. Высокотемпературный электрохимический синтез силицидов металлов VI-A группы в галогенидно-оксидных расплавах / В. В. Малышев, Р. В. Куприна, И. А. Новоселова, Т. В. Верховлюк // Журнал неорганической химии. ― 1996. ― Т. 41, № 12. ― С. 1992‒1996.

18. Баньковская, И. Б. Термическая стабильность некоторых стеклокерамических композиций при 1400 °С. Температуроустойчивые покрытия : тр. 11-го Всесоюз. совещания по жаростойким покрытиям, Ленинград, 31 мая ‒ 2 июня 1983 г. / И. Б. Баньковская, М. В. Сазонова. ― Л. : Наука, 1985. ― С. 86‒91.


Supplementary files

For citation: Ban’kovskaya I.B., Kolovertnov D.V., Sazonova M.V. Temperature coefficient of linear expansion of glass-ceramic materials based on MoSi2. NOVYE OGNEUPORY (NEW REFRACTORIES). 2023;(7):38-41. https://doi.org/10.17073/1683-4518-2023-7-38-41

Views: 178

Refbacks

  • There are currently no refbacks.


ISSN 1683-4518 (Print)