High-temperature propagate compounds of ceramomatic composite materials reinforced with carbon fibers, with similar and other carbon-containing materials
https://doi.org/10.17073/1683-4518-2022-2-32-44
Abstract
An analysis of the use of soldering, reaction and gas-phase binding methods and gluing to obtain high-temperature suprame compounds of carbidremium ceramomatic composite materials (CMCM) with similar materials, as well as carbon-carbon materials (CCM) and graphite is carried out. The main problems with the compounds of CMCM with carbon-containing materials associated with the poor wettability of the CMCM melt melts, a significant difference between TCRC kmk and soldering, with the formation of substances with high hardness and fragility in the connecting layer. An analysis of the practical experience of applying soldering methods, reaction and gas-phase binding, gluing for the Cf/SiC connection with various carbon-containing materials. The most typical compositions of solders and adhesives, technological modes of the compound processes are considered. It is shown that these technologies make it possible to create reliable and durable compounds of parts from kmk and various types of carbon-containing materials. Ill. 7. Ref. 61. Tab. 1.
About the Authors
V. I. KulikRussian Federation
A. S. Nilov
Russian Federation
E. A. Bogachev
Russian Federation
References
1. Hanbook of ceramic composites ; ed. by P. Narottam. ― Bansal : Boston, Dordrecht, London : Kluver Academic Publishers, 2005. ― 554 p.
2. Гаршин, А. П. Анализ современного состояния и перспектив коммерческого применения волокнистоармированной карбидкремниевой керамики / А. П. Гаршин, В. И. Кулик, А. С. Нилов // Новые огнеупоры. ― 2012. ― № 2. ― С. 43‒52.
3. Mergia, K. Joining of C f/C and Cf/SiC composites to metals / K. Mergia // Nanocomposites with unique properties and applications in medicine and industry ; еd. by Dr. John Cuppoletti. InTech, 2011. ― P. 239‒266.
4. Zhang, K. Joining of Cf/SiC ceramic matrix composites : a review / K. Zhang, L. Zhang, R. He // Advances in Materials Science and Engineering. ― 2018. ― Vol. 2018. ― Article ID 6176054.
5. Кулик, В. И. Методы пайки для получения не разъемных соединений керамических композиционных материалов с металлами (Обзорная статья)/ В. И. Кулик, А.С. Нилов, Е. А. Богачев, Н. В. Ларионов // Новые огнеупоры. ― 2021. ― № 4. ― С. 42‒52.
6. Гаршин, А. П. Современные технологии полу чения волокнисто-армированных композиционных материалов с керамической огнеупорной матрицей (Обзор) / А. П. Гаршин, В. И. Кулик, С. А. Матвеев, А. С. Нилов // Новые огнеупоры. ― 2017. ― № 4. ― С. 20‒35.
7. Morozumi, S. Bonding mechanism between silicon carbide and thin foils of reactive metals / S. Morozumi, M. Endo, M. Kikuchi // Journal of Materials Science. ― 1985. ― Vol. 20, № 11. ― P. 3976‒3982.
8. Fan, X. M. Oxidation behavior of C/SiC‒Ti3SiC2 at 800‒1300 оC in air / X. M. Fan, X. W. Yin, Y. Z. Ma [et al.] // J. Eur. Ceram. Soc. ― 2016. ― Vol. 36. ― P. 2427‒2433.
9. Dong, H. Y. Joining of SiC ceramic-based materials with ternary carbide Ti3SiC2 / H. Y. Dong, S. J. Li, Y. Y. Teng, W. Ma // Materials Science and Engineering: B. ― 2011. ― Vol. 176, № 1. ― P. 60‒64.
10. Fan, D. Correlation between microstructure and mechanical properties of active brazed Cf/SiC composite joints using Ti‒Zr‒Be / D. Fan, J. Huang, X. Sun [et al.] // Materials Science and Engineering: A. ― 2016. ― Vol. 667. ― P. 332‒339.
11. Wang, J. Effects of bonding temperature on the microstructures and mechanical properties of the C/C‒ Cf/SiC composite joint prepared by in situ hot-press diffusion bonding using Ti‒Si‒C compound as interlayer / J. Wang, Y. Xiong, H. Li [et al.] // Materials Research Express. ― 2019. ― Vol. 6, № 11. ― Аrticle № 115620.
12. Tokita, M. Spark plasma sintering (SPS) method, systems, and applications / M. Tokita // Handbook of Advanced Ceramics. ― 2013. ― Ch. 11.2.3. ― P. 1149‒1177.
13. Rizzo, S. Joining of C/SiC composites by spark plasma sintering technique / S. Rizzo, S. Grasso, M. Salvo [et al.] // J. Eur. Ceram. Soc. ― 2014. ― Vol. 34, № 4. ― P. 903‒913.
14. Tatarko, P. Flash joining of CVD-SiC coated C f/SiC composites with a Ti interlayer / P. Tatarko, S. Grasso, T. G. Saunders [et al.] // J. Eur. Ceram. Soc. ― 2017. ― Vol. 37. ― P. 3841‒3848.
15. Zhao, X. Improved shear strength of SiC-coated 3D C/SiC composite joints with a tailored Ti‒Si‒C interlayer / X. Zhao, L. Duan, Y. Wang // J. Eur. Ceram. Soc. ― 2018. ― Vol. 39, № 4. ― P. 788‒797.
16. Tatarko, P. Joining of CVD-SiC coated and uncoated fibre reinforced ceramic matrix composites with pre-sintered Ti3SiC2 MAX phase using Spark Plasma Sintering / P. Tatarko, V. Casalegno, C. Hu [et al.] // J. Eur. Ceram. Soc. ― 2016. ― Vol. 36. ― Р. 3957‒3967.
17. Zhao, X. Fast-diffusion joining of SiC-coated threedimensional C/SiC composites with a Mo‒W‒Mo interlayer by spark plasma sintering / X. Zhao, L. Duan, W. Liu, Y. Wang // Ceram. Int. ― 2019. ― Vol. 45, № 17. ― Part B. ― P. 23111‒23118.
18. Zhao, X. Fast interdiffusion and Kirkendall effects of SiC-coated C/SiC composites joined by a Ti‒Nb‒Ti interlayer via spark plasma sintering / X. Zhao, L. Duan, Y. Wang // J. Eur. Ceram. Soc. ― 2019. ― Vol. 39, № 5. ― P. 1757‒1765.
19. Zhao, X. Shear strength enhancement of SiC-coated 3D C/SiC composite joints with a Ni‒Ti‒Nb multiinterlayer by interfacial microstructure tailoring / X. Zhao, L. Duan, W. Liu, Y. Wang // J. Eur. Ceram. Soc. ― 2019. ― Vol. 39, № 16. ― P. 5473‒5478.
20. Fernie, J. A. Joining of engineering ceramics / J. A. Fernie, R. A. L. Drew, K. M. Knowles // International Materials Reviews. ― 2009. ― Vоl. 54, № 5. ― P. 283‒331.
21. Todt, A. Joining of glassy carbon with a C/C‒SiC composite by brazing for an Innovative high temperature sensor / A. Todt, K. Roder, D. Nestler, B. Wielage // Ceramic Transactions. ― 2014. ― Vol. 248. ― P. 661‒667.
22. Chen, B. Microstructure and strength of Cf/SiC joints with Ag‒Cu‒Ti brazing fillers / B. Chen, H. P. Cheng, W. Mao [et al.] // Journal of Materials Engineering. ― 2010. ― Vol. 329. ― P. 27‒31.
23. Xiong, H. P. Joining of Cf/SiC composite with Pd‒ Co‒V brazing filler / H. P. Xiong, B. Chen, W. Mao, X.-Н. Li // Welding in the World. ― 2012. ― Vol. 56, № 1/2. ― Р. 76‒80.
24. Xiong, H.-P. Joining of Cf/SiC composite with a Cu‒ Au‒Pd‒V brazing filler and interfacial reactions / H.-P. Xiong, B. Chen, Y. Pan, H.-Sh. Zhao // J. Eur. Ceram. Soc. ― 2014. ― Vol. 34, № 6. ― P. 1481‒1486.
25. Li, W.-W. Reactive brazing Cf/SiC to itself and to Mo using the NiPdPtAu-Cr filler alloy / W.-W. Li, B. Chen, H.P. Xiong, W.-J. Zou // J. Eur. Ceram. Soc. ― 2017. ― Vol. 37, № 13. ― Р. 3849‒3859.
26. Chen, J. In situ-strengthened C/SiC joint brazed with Cu-based active filler and its performance / J. Chen, S. Dong, X. Zhang // International Journal of Applied Ceramic Technology. ― 2015. ― Vol. 12, № s3. ― Р. E197‒E207.
27. Chen, B. Joining of Cf/SiC composite with AuNi(Cu)‒ Cr brazing fillers and interfacial reactions / B. Chen, H.-P. Xiong, X. Wu, Y.-Y. Cheng // Welding in the World. ― 2016. ― Vol. 60, № 4. ― P. 813‒819.
28. Tong, Q. Liquid infiltration joining of 2D C/SiC / Q. Tong, L. Cheng // Composite Science and Engineering of Composite Materials. ― 2006. ― Vol. 13. ― P. 31‒36.
29. Patent WO 2011/113760 Al. Method of joining parts made of SiC-based materials by non-reactive brazing with addition of a reinforcement, brazing compositions and joint and assembly that are obtained by such a method / V. Chaumat, J. Henne. Опубл. 22.09.2011.
30. Patent US 8678269-B2. Method for assembling, joining parts made of SiC-based materials by nonreactive brazing, brazing compositions, and joint and assembly obtained by said method / V. Chaumat, J.-F. Henne, Miloud-Ali N. Опубл. 25.03.2014.
31. Patent US 7318547 B2. Method for assembling parts made of materials based on SiC by non-reactive refractory brazing, brazing compositions, and joint and assembly obtained by said method / A. Gasse. Опубл. 15.01.2008.
32. Riccardi, B. Joining of SiC based ceramics and composites with Si–16Ti and Si–18Cr eutectic alloys / B. Riccardi, C. A. Nannetti, J. Woltersdorf [et al.] // International Journal of Materials and Product Technology. ― 2004. ― Vol. 20. ― Р. 440‒451.
33. Patent US 2006/0006212. Method of brazing composite materials parts sealed with a silicon-based composition / J. Thebault, C. Bouquet. Опубл. 12.01.2006.
34. Gianchandani, P. K. Pressure-less joining of C/SiC and SiC/SiC by a MoSi2/Si composite / P. K. Gianchandani, V. Casalegno, F. Smeacetto, M. Ferraris // International Journal of Applied Ceramic Technology. ― 2017. ― Vol. 14, № 3. ― P. 305‒312.
35. Smeacetto, F. Ytterbium disilicate-based glassceramic as joining material for ceramic matrix composites / F. Smeacetto, F. D’Isanto, V. Casalegno [et al.] // J. Eur. Ceram. Soc. ― 2021. ― Vol. 41. ― P. 1099‒1106.
36. Bacos, M. P. Carbon–сarbon composites: oxidation behavior and coatings protection / M. P. Bacos // Journal de Physique IV. ― 1993. ― Vol. 3. ― P. 1895‒1903.
37. Fu, Q. A multi-interlayer LMAS joint of C/C‒SiC composites and LAS glass ceramics / Q. Fu, F. Zhao, H. Li [et al.] // Journal of Materials Science & Technology. ― 2015. ― Vol. 31. ― Р. 467‒472.
38. Ferraris, M. Joining of machined SiC/SiC composites for thermonuclear fusion reactors / M. Ferraris, M. Salvo, V. Casalegno [et al.] // Journal of Nuclear Materials. ― 2008. ― Vol. 375. ― Р. 410‒415.
39. Katoh, Y. Microstructure and mechanical properties of low-activation glass-ceramic joining and coating for SiC/SiC composites / Y. Katoh, M. Kotani, A. Kohyama [et al.] // Journal of Nuclear Materials. ― 2000. ― Vol. 283. ― Р. 1262‒1266.
40. Salvo, M. Advanced manufacturing routes for metal/composite components for aerospace / М. Salvo // ECCM16 ‒ 16TH European conference on composite materials, Seville, Spain, 22‒26 June 2014. ― Conference Paper, 2014. ― 6 р.
41. Krenkel, W. Carbon fiber reinforced CMC for highperformance structures / W. Krenkel // International Journal of Applied Ceramic Technology. ― 2004. ― Vol. 1, № 2. ― Р. 188‒200.
42. Wu, X. Joining of the Cf/SiC composites by a one-step Si infiltration reaction bonding / X. Wu, B. Pei, Y. Zhu, Zh. Huang // Materials Characterization. ― 2019. ― Vol. 155. ― Article ID 109799.
43. Singh, M. Affordable, robust ceramic joining technology (ARCJoinT) for high temperature applications. In Proceedings of Joining of Advanced and Specialty Materials / M. Singh // ASM International, Materials Park, OH, 1998. ― Р. 1‒5.
44. Пат. 2604530 Российская Федерация. Композиция для соединения керамических композиционных материалов на основе карбида кремния / Каблов Е. Н., Гращенков Д. В., Солнцев С. С., Ваганнова М. Л., Сорокин О. Ю. ― № 2015145235/03 ; заявл. 21.10.15 ; опубл. 10.12.16, Бюл. № 34.
45. Пат. 2415822 Российская Федерация. Способ неразъемного соединения деталей / Богачев Е. А., Лахин А. В., Тимофеев А. Н., Удинцев П. Г., Чунаев В. Ю. ― № 2008140680/03 ; заявл.15.10.08 ; опубл. 10.04.2011, Бюл. № 10.
46. Разина, А. С. Выбор состава металлоперехода для камеры сгорания жидкостного ракетного дви гателя малой тяги / А. С. Разина, Н. П. Асташева // Информационно-технологический вестник. ― 2018. ― № 2 (16). ― С. 149‒155.
47. Bogachev, E. A. MMS Technology: first results and prospects / E. A. Bogachev, A. V. Lahin, A. N. Timofeev // Ceramic Transactions. ― 2014. ― Vol. 248. ― P. 243‒253.
48. Srivastava, V. K. Adhesive bonded single lap and over-lap joints of C/C, C/C-SiC composites and titanium alloy / V. K. Srivastava, S. Singh // Journal of Mechanical Engineering Research. ― 2011. ― Vol. 3, № 5. ― Р. 162‒167.
49. Пат. 2473582 Российская Федерация. Клейкомпаунд / Сыздыков Е. К., Жаворонков А. В., Логинов А. И., Никитин В. В., Удинцев П. Г., Чунаев В. Ю., Воробьев А. С., Руденко Д. А. ― № 2011145927/05 ; заявл. 11.11.11 ; опубл.: 27.01.2013, Бюл. № 3.
50. Chen, X. The effect of high-treatment on the strength of C/C‒SiC joints / X. Chen, S. Li, Z. Chen, N. Wen // Journal of Material Science. ― 2011. ― Vol. 46. ― Р. 707‒714.
51. Chen, X. Joining of C/C‒SiC using boron-modified phenolic resin with SiO2 and B4C additives / X. Chen, S. Li, Zh. Chen // Materials at High Temperatures. ― 2011. ― Vol. 28, № 1. ― Р. 28‒32.
52. Li, S. The effect of high temperature heat-treatment on the strength of C/C to C/C–SiC joints / S. Li, X. Chen, Zh. Chen // Carbon. ― 2010. ― Vol. 48, № 11. ― P. 3042‒3049.
53. Гладких, С. Н. Термо- и жаростойкие клеи для соединения углеродных и керамических материалов / С. Н. Гладких, М. Г. Мокрушин // Клеи. Герметики. Технологии. ― 2010. ― № 3. ― С. 6‒12.
54. Гладких, С. Н. Новые клеи разработки ОАО «КОМПОЗИТ» для изделий ракетно-космической техники / С. Н. Гладких, А. Э. Дворецкий, А. И. Вялов // Адгезионные материалы : труды научно-технической конференции. ― Москва, ВИАМ, 27 апреля 2016 года, 2016. ― 13 с.
55. Сосунов, С. А. Термостойкие соединения углеродных материалов фенолофурфуролоформальдегидными клеями / С. А. Сосунов, Г. В. Комаров, С. В. Бухаров, Г. А. Кравецкий // Пластические массы. ― 2003. ― № 9. ― C. 40, 41.
56. Клей СТЭП-ТК2 [Электронный ресурс] https:// npkstep.ru/wp-content/uploads/2016/07/STEP-TK2NEW.pdf. Дата обращения. 20.12.2020.
57. Liu, H.-L. Technique of joining of Cf/SiC composite via preceramic silicone polysilazane and joining properties / H.-L. Liu, C.-Y. Tian, M.-Z. Wu // Chinese Journal of Nonferrous Metals. ― 2008. ― Vol. 18, № 2. ― Р. 278‒281.
58. Liu, H. Joining of C f/SiC ceramic matrix composite using SiC‒Si3N4 preceramic polymer / H. Liu, S. Li, Z. Chen // Materials Science Forum. ― 2005. ― Vol. 475. ― Р. 1267‒1270.
59. Lu, Y. W. Online-joining of C/SiC‒C/SiC via precursor infiltration and pyrolysis process / Y. W. Lu, Y. D. Zhang, H. F. Hu, Ch. R. Zhang // Key Engineering Materials. ― 2008. ― Vol. 368‒372. ― P. 1044‒1046.
60. Zhang, Y. D. Online-joining of C/SiC‒C/SiC via slurry reaction and precursor infiltration and pyrolysis process with C/SiC pins / Y. D. Zhang, H. F. Hu, Ch. R. Zhang, G. D. Li // Key Engineering Materials. ― 2012. ― Vol. 531/532. ― Р. 135‒140.
61. Петрова, А. П. Термостойкие клеи / А. П. Петрова. ― М. : Химия, 1977. ― 152 с.
Supplementary files
For citation: Kulik V.I., Nilov A.S., Bogachev E.A. High-temperature propagate compounds of ceramomatic composite materials reinforced with carbon fibers, with similar and other carbon-containing materials. NOVYE OGNEUPORY (NEW REFRACTORIES). 2022;(2):32-44. https://doi.org/10.17073/1683-4518-2022-2-32-44
Refbacks
- There are currently no refbacks.