Significance of AlN and TiN coatings for controlled transformation of stress state of : Si3N4-TiC ceramics surface layer under force loading conditions
https://doi.org/10.17073/1683-4518-2022-3-62-68
Abstract
About the Authors
V. V. KuzinRussian Federation
S. N. Grigor'ev
Russian Federation
M. A. Volosova
Russian Federation
M. Yu. Fedorov
Russian Federation
References
1. Kuzin, Valery V. A new generation of ceramic tools / Valery V. Kuzin, Sergey N. Grigor’ev, David R. Burton, Andre D. Botako // Proceedings of the 10th International Conference on Manufacturing Research (ICMR), 2012. ― Р. 523‒528.
2. Lube, Tanja. Indentation crack profiles in silicon nitride / Tanja Lube // J. Eur. Ceram. Soc. ― 2001. ― Vol. 12, № 2. ― Р. 211‒218.
3. Kadin, Yuri. In-situ observation of crack propagation in silicon nitride ceramics / Yuri Kadin, Stefan Strobl, Charlotte Vieillard [et al.] // Procedia Structural Integrity. ― 2017. ― Vol. 7. ― Р. 307‒314.
4. Like, Qiu. Study on toughness mechanism of ceramic cutting tools / Qiu Like, Li Xikun, Qiu Guanming, Ma Weimin // Journal of Rare Earths. ― 2007. ― Vol. 25, № 2. ― Р. 309‒316.
5. Peillon-Cluzel, F. Study of the secondary phase in gas pressure sintered Si3N4 (relation composition-toughness) / F. Peillon-Cluzel, F. Thevenot, T. Epicier // Int. J. Refract. Met. Hard Mater. ― 2001. ― Vol. 19, № 4‒6. ― Р. 419‒424.
6. Guo, Shuqi. Hot-pressed Si3N4 ceramics with Lu2O3 additives: Grain-boundary phase and strength / Shuqi Guo, Naoto Hirosaki, Yoshinobu Yamamoto [et al.] // Mater. Sci. Eng., A. ― 2005. ― Vol. 408, № 1/2. ― Р. 9‒18.
7. Zou, Linhua. The measurement and characterization of the interfacial toughness of Si3N4/BN composites by a three-point bending test / Linhua Zou, Yong Huang, Ruifeng Chen [et al.] // J. Eur. Ceram. Soc. ― 2003. ― Vol. 23, № 11. ― Р. 1987‒1996.
8. Carrapichano, J. M. Tribological behaviour of Si3N4– BN ceramic materials for dry sliding applications / J. M. Carrapichano, J. R. Gomes, Rui F. Silva // Wear. ― 2002. ― Vol. 253, № 9‒10. ― Р. 1070‒1076.
9. Kuzin, V. V. Wear of tools from nitride ceramics when machining nickel-based alloys / V. V. Kuzin, M. A. Volosova, M. Yu. Fedorov // J. Frict. Wear. ― 2013. ― Vol. 34, № 3. ― Р. 199‒203. [Кузин, В. В. Износ инструментов из нитридной керамики при обработке никелевых сплавов / В. В. Кузин, М. А. Волосова, М. Ю. Федоров // Трение и износ. ― 2013. ― Т. 34, № 3. ― С. 265‒271.]
10. Finkeldei, Daniel. End milling of Inconel 718 using solid Si3N4 ceramic cutting tools / Daniel Finkeldei, Marcus Sexauer, Friedrich Bleicher // Procedia CIRP. ― 2019. ― Vol. 81. ― Р. 1131‒1135.
11. Tian, Xianhua. Performance of Si3N4 / (W, Ti) C graded ceramic tool in high-speed turning iron-based superalloys / Xianhua Tian, Jun Zhao, Xinya Wang [et al.] // Ceram. Int. ― 2018. ― Vol. 44, № 13. ― Р. 15579‒15587.
12. Kuzin, V. Tool life and wear mechanism of coated Si3N4 ceramic tools in turning grey cast iron / V. Kuzin, S. Grigoriev // Key Eng. Mater. ― 2014. ― Vol. 581. ― Р. 14‒17.
13. Brovkova, M. B. The main directions for increasing the tool life of a metal cutting tool with modified working parts / M. B. Brovkova, V. V. Martynov, E. S. Pleshakova // Journal of Machinery Manufacture and Reliability. ― 2020. ― Vol. 49, № 2. ― P. 137‒143.
14. Liu, Wei. PVD-CrAlN and TiAlN coated Si3N4 ceramic cutting tools‒1. Microstructure, turning performance and wear mechanism / Wei Liu, Quanquan Chu, Junjie Zeng [et al.] // Ceram. Int. ― 2017. ― Vol. 43, № 12. ― Р. 8999‒9004.
15. Grigoriev, S. The stress-strained state of ceramic tools with coating / S. Grigoriev, V. Kuzin, D. Burton, A. D. Botako // Proceedings of the 37th International MATADOR Conference, 2013. ― P. 181‒184.
16. Liu, Wei. Preparation and properties of TiAlN coatings on silicon nitride ceramic cutting tools / Wei Liu, Quanquan Chu, Rongxuan He [et al.] // Ceram. Int. ― 2018. ― Vol. 44, № 2. ― Р. 2209‒2215.
17. Blugan, G. Si3N4‒TiN based micro-laminates with rising R-curve behavior / G. Blugan, R. Dobedoe, M. Lugovy [et al.] // Composites. Part B: Engineering. ― 2006, ― Vol. 37, № 6. ― Р. 459‒465.
18. Liu, Wei. PVD-CrAlN and TiAlN coated Si3N4 ceramic cutting inserts‒2. High speed face milling performance and wear mechanism study / Wei Liu, Quanquan Chu, Junjie Zeng [et al.] // Ceram. Int. ― 2017. ― Vol. 43, № 12. ― Р. 9488‒9492.
19. Ševeček, Oldřich. Assessment of crack-related problems in layered ceramics using the finite fracture mechanics and coupled stress-energy criterion / Oldřich Ševeček, Michal Kotoul, Dominique Leguillon [et al.] // Procedia Structural Integrity. ― 2016. ― Vol. 2. ― Р. 2014‒2021.
20. Lugovy, M. Apparent fracture toughness of Si3N4-based laminates with residual compressive or tensile stresses in surface layers / M. Lugovy, V. Slyunyayev, N. Orlovskaya [et al.] // Acta Materialia. ― 2005. ― Vol. 53, № 2. ― Р. 289‒296.
21. Sun, X. Computer-aided three-dimensional ceramic product design / X. Sun, X. Yang, B. Song, X. Liu // Computer-Aided Design and Applications. ― 2022. ― Vol. 19, № S3. ― P. 97‒107.
22. Kuzin, V. V. Basic framework for computer-aided engineering of polished ceramic surface layers / V. V. Kuzin, S. N. Grigor’ev, M. A. Volosova // Refract. Ind. Ceram. ― 2020. ― Vol. 61, № 3. ― P. 349‒354. [Кузин, В. В. Основы компьютерной инженерии поверхностного слоя шлифованной керамики / В. В. Кузин, С. Н. Григорьев, М. А. Волосова // Новые огнеупоры. ― 2020. ― № 6. ― С. 64‒69.]
23. Kuzin, V. Method of investigation of the stress-strain state of surface layer of machine elements from a sintered nonuniform material / V. Kuzin, S. Grigoriev // Applied Mechanics and Materials. ― 2014. ― Vol. 486. ― Р. 32‒35.
Supplementary files
For citation: Kuzin V.V., Grigor'ev S.N., Volosova M.A., Fedorov M.Y. Significance of AlN and TiN coatings for controlled transformation of stress state of : Si3N4-TiC ceramics surface layer under force loading conditions. NOVYE OGNEUPORY (NEW REFRACTORIES). 2022;(3):62-68. https://doi.org/10.17073/1683-4518-2022-3-62-68
Refbacks
- There are currently no refbacks.